Any thoughts on this plan for an old stone (slate & lime mortar) - the back wall is 600mm below ground level - walls need to breath and condensation minimised ...
Walls preped back to stone and raked out
Back wall tanking (tank up to 1m from floor): 12mm s&c renderwith SBR; 2mm Newton 107F brushed on
Back wall above tanking: 15mm Limelite renovating plaster scratch coat; use mesh at joint with tanking
Back wall to finish: Limelite Easy bond; 10mm Limelite renovating plaster; Limelite high impact finish
Other walls (no tanking): 15mm Limelite renovating plaster scratch coat; 10mm Limelite renovating plaster second coat; Limelite high impact finish
What would you do?
Walls preped back to stone and raked out
Back wall tanking (tank up to 1m from floor): 12mm s&c renderwith SBR; 2mm Newton 107F brushed on
Back wall above tanking: 15mm Limelite renovating plaster scratch coat; use mesh at joint with tanking
Back wall to finish: Limelite Easy bond; 10mm Limelite renovating plaster; Limelite high impact finish
Other walls (no tanking): 15mm Limelite renovating plaster scratch coat; 10mm Limelite renovating plaster second coat; Limelite high impact finish
What would you do?