apologies if this topic has already been posted. I and 3 of my lads have recently skimmed 600sqm of plasterboard walls on a site in Glasgow. A week after i finished I was called back. 70-80% of the walls have all peaked on the joints. All framing is metal stud, there are little to no peaks at the top or bottom of the joints, from 500mm onwards from top to bottom getting worse in the centre, has anyone ever seen this ?
apologies if this topic has already been posted. I and 3 of my lads have recently skimmed 600sqm of plasterboard walls on a site in Glasgow. A week after i finished I was called back. 70-80% of the walls have all peaked on the joints. All framing is metal stud, there are little to no peaks at the top or bottom of the joints, from 500mm onwards from top to bottom getting worse in the centre, has anyone ever seen this ?