Hello lads,
Done some 1.5mm silicone render, 1st time, small area. Went on fine, floated with plastic float, come back next day and really tiny cracks around the grain across the whole area.
I picked up the supplies off a polish builders merchant. Couldn't read the instructions, so mixed up the bucket with paddle mixer and off I went. Looks like I'ved buggered up somewhere!
Any help appreciated. I'm reading some guys put water in the bucket? Prime the area again? I've primed it once already, is two coats recommended in this weather?
What can I do to sort out the cracking/crazing in the current patch I've done?
Cheers
Done some 1.5mm silicone render, 1st time, small area. Went on fine, floated with plastic float, come back next day and really tiny cracks around the grain across the whole area.
I picked up the supplies off a polish builders merchant. Couldn't read the instructions, so mixed up the bucket with paddle mixer and off I went. Looks like I'ved buggered up somewhere!
Any help appreciated. I'm reading some guys put water in the bucket? Prime the area again? I've primed it once already, is two coats recommended in this weather?
What can I do to sort out the cracking/crazing in the current patch I've done?
Cheers