Hi lads hope your all well and working hard.
Finally had my first go of k rend on my garage last week, scratched with base coat and mesh derbeyd and topped with k rend and derbeyd that too. gave it a day then scratched back overall it looks well...90% however there are a few smooth lines and patches that won't scratch up to the same as the rest. These stand out quite a bit and are pissing me off as I put so much effort Ito getting It spot on
I've put a rule up over these lines and there doesn't seem to be any hollows
Any idea what's caused these where I've went wrong
Would I be able to Krend over Krend?
Any help would be much appreciated cheers fellas
Finally had my first go of k rend on my garage last week, scratched with base coat and mesh derbeyd and topped with k rend and derbeyd that too. gave it a day then scratched back overall it looks well...90% however there are a few smooth lines and patches that won't scratch up to the same as the rest. These stand out quite a bit and are pissing me off as I put so much effort Ito getting It spot on
I've put a rule up over these lines and there doesn't seem to be any hollows
Any idea what's caused these where I've went wrong
Would I be able to Krend over Krend?
Any help would be much appreciated cheers fellas