depends on the size of panel, by the time youve patched it and messed around with it, you could have just gone over it again.
if its anything less than a 1.5mm grain, id recon it will show when the sun sits on it.
Unless its piss wet it probably won't blend back in. Might be best to cut your losses and fill in the missing/washed off areas with acrylic again taking care not to double up on the joint. Once dry go over the whole area again. If anything acrylic over acrylic is nicer to apply as the second coat grips the grain of the first coat but still looks the same(maybe slightly better actually).