Got a small scratch render job to do in a couple weeks onto block work. Now I've done a fair bit of it, but when I worked for a firm and they just ordered it by the lorry load. I'm going to use base coat then top coat the next day. Customer wants 8mm base and 10mm scraped back to 8mm top coat. The job is roughly 30m2. After reading up a bit about coverage I'm guessing I may be a little short. I've told them to order 25 bag as I thought it was 1.5-2m2 per bag?

Edited to say 25 bag of each
 
Use mesh cloth if less then 7 newton over the lot ,but stress mesh as normal if it 7 newton
 
Well i done this job on friday&saturday. Must say im really happy with it as ive not done any k rend for well over 2 years, this being the first one on my own. Only 1 elevation but customer really happy and ive got a full house skim outta this job too. Ended up basecoating 6mm and top10mm. 20 base & 28 top was more than enough. Customers sending me pictures when scaffold is dropped do might fire them up.

Thanks for thr advice chaps
 
Status
Not open for further replies.
Top