Hello I'm a lime plasterer/renderer from the west Midlands. How are my fellow brethren doing across the country?
 
Welcome mate! One the question no one could give an answer was do use the same ratio3:1 for harl,scratch,float and top coat? Maybe you could shed a light on this one?
 
Hello, I use a ratio of 1.5 sand to 1 lime for base and 2 or 3 :1 for top coat depending on if the area is subject to hard weathering.
 