A little bonding in the first coat with the multi then second coat after 20 mins with multi, it trowels in perfect like glass. They said do it this way anymore, even if it takes longer!
I normally use a light coat of skim and few handfuls of bonding when skimming over old walls that have the green stuff painted on, for first coat then level it twice and then second coat, the job I am on wants me to use hard wall and skim instead of bonding for first coat, never seen anybody...