on sunday. 550m of plain face render. now i wen i have done it b4 its been deliverd now we gotta mix our own. whats the best mix for scratch and best for top coat. also do you guys use lime in you mix. £22m labour only. now thats a price worth traveling for ;D
 
4 to 1 scratch with waterproofer + plasticiser , top coat 5 to 1 with shovel of lime plus plasticiser luvly jubly.
 
i have been told not to put water proofer in the scratch and just to wet thye wall down loads before topping. would this not work
 