any help on this one would be great :), i have just skimmed a room board work on dot and dab walls and notice that the joint are cracking a little, there all taped up with fibre tape skim skim didnt go off very fast, 2 or 3 day to dry out thick first coat tight sec 3mm max, i am now think of...
Spoke to cementone tech team today about using their wintaplas frostproofer. They said you cant use waterproofer with the frostproofer, so wondered how do i go about waterproofing the wall and how to protect it from the frost. Any tips on rendering outside this time of year and what product are...
hi , i have took off wallpaper and find that i think it old lime plaster, it not render/bonding or hardwall so im thinking lime down stair is not painted but upstairis is, she wants to keep the skirting so it got to be a thin coat plaster ( multi finish is not good with lime i have hear so im...
hi guys, looking at doing some free work for experience with k render / pral m , i can render s/c bead up , mix , just need abit of training and though this would be the best place to ask cheer tony
what the best ratio for mixing render i do 1st coat 4/1 2nd coat 4sand 3/4 cement 1/4 lime was taught this way, what do you guys think is it right and what the best sand cheer
hi guys, just on a job and the bulider has used quinn lite block outside his say there fine to render on but i know different, i need a solution do i render aid it/ sbr slurry/ or buliding paper and eml any ideas