I've just mastered the flex no tigers ,no bumps .i used the trowel before but had problems but this time I think from past use it wore in abit and I used no water at all well about a tea spoons worth to clean the edges and I jumped on it soaking wet after speed skim and let it go hard and trowel...
Used one for first time today .Brilliant ! Always used the grey one thought it was good but the blue is way better and rules render up nice and flat found the grey ones would bend with the wall a bit but yeh blue speed skim living the dream :RpS_cool:
Hi guys ,I'm starting s+c moz on a house that's old shitty render that's all sound so I've render gripped it today was gona do 5.1 very little waterproof and bed fibre glass mesh in scratch then leave to dry fully out and top with a 6.1.1 lime with half rapid cement and half normal and just feb...
Had a big site on a while back had to knock out the houses quick ,we was scraping all the linings but then had the decorators moaning that we was fooking them up by chipping them and they had to fill them ( they were cheap shite linings anyway) now common sense kicked in we put duct tape around...
Don't get on with the nela sf but get on with refina plastic ??
problems I have with nela - rides over bumps ,leaves tiger stripes
with refina plastic don't get any of that same timings used and there both flexible trowels and nela should be better if anything .
i always 1st trowel with mt...