There was loads of mess every day but the company has been round to inspect and agrees it’s not been done right and reckon they will come back in 2 to 3 weeks to put it right. My only concern is that they reckon they can put it right in ONE day!!!!
I contacted the K Rend company and their technical dept put it down to too much scratching and thinning out the render. They did say to wait 4 or 5 weeks until it’s properly cured and then new K render can be applied. I’ve attached a few photos.
Hi,
My house has just been K rendered and the finish is not consistent across the wall surface and the base coat is still showing through in various places.
Can this be easily fixed and patched up as I am struggling to get the firm to return and put this right.
Would appreciate some advice.