Looks like he hasn’t dampened down the substrate before applying the hard wall
Also when putting hardwall on its better to apply in two or three layers as it kills the suction and stops it drying out to fast
The skim looks like he has left the hardwall to long and the suction has got him...
Thanks zolco for the informative reply
Them rates look shocking to me
I know a local firm that done airless on a job I tendered for .
The top floor was airless and the other 2 floors was skimmed due to the poor quality of application and finish but it was end of winter so inexperience...
Ok thanks Zolco
So more time on preparation and flattening walls
Most reskims we do the walls are really bad so not sure how much quicker airless would be
Do you think it’s a better system or only on certain jobs?
Was looking into airless for a couple of full reskims
Would you advise against it ?
Is it something I could just rent the tools and have a go at without going on a course befog
In the same boat I’m 42 been doing since 17
Speed is slowly going and it’s getting harder mentally and physically
I got a few people that work for me so not to bad
That’s why so intrested in airless plaster as it looks less demanding on the body