Recent content by shilo

  1. S

    Powdery New Render (dried to quickly in hot / direct sunshine maybe???)

    thanks for the replies. I'm guessing Febond PVA isn't up to the job then?
  2. S

    Powdery New Render (dried to quickly in hot / direct sunshine maybe???)

    Well....the scratch coat coming off :RpS_crying:. Any tips on the mix and preparation of the substrate. I think the bricks are concrete commons but after 40 years of curing have hardened to engineering strength. The wall also has a high degree of suction. They were previously rendered and dashed...
  3. S

    Powdery New Render (dried to quickly in hot / direct sunshine maybe???)

    Great:RpS_mad: thanks for all the reples
  4. S

    Powdery New Render (dried to quickly in hot / direct sunshine maybe???)

    Sorry for the lack of responding...been away for 2 days. So i'm guessing it all needs to come back off then?
  5. S

    Powdery New Render (dried to quickly in hot / direct sunshine maybe???)

    It looked like the sand I used to use when laying bricks from a local builders merchant. As far as I know it was a 4:1 mix with water proofer.
  6. S

    Powdery New Render (dried to quickly in hot / direct sunshine maybe???)

    Hi, I’m not a plasterer but I was a bricklayer in a previous life before a couple of prolapsed discs ended that. So I’ve got some knowledge of mortar but not in the spreading department. Anyway.....I’m currently having my bungalow renovated and the external render is being renewed by...
Top