    1.5mm silicone render, cracking all over

    How’s about an agree to respect each other’s views and appreciate we may take a different approach to get the same end result ...... a decent job. If anything you owe my missus an apology as she just had to eat burnt shepherds pie as I was busy giving it large and forget the oven was on.
  2. Mr White

    1.5mm silicone render, cracking all over

    To be competitive we will have to move with the market, what else can I do. What really annoys me is when we go to a manufacturer training day my labourer (thick as f**k) is twice as fast and twice as neat as the plasterers there, my labourer cannot plaster btw.
  3. Mr White

    1.5mm silicone render, cracking all over

    On that note, I am fed up of getting phone calls and looking at jobs that have been f**k*d up and not done correctly. On here and in real life. That’s why I like to try and give some good info to avoid people getting taken for £0000 and hopefully encourage people to look into more than just the...
  4. Mr White

    1.5mm silicone render, cracking all over

    No, our system is 1 spray followed by 1 takes excess off with steel trowel then 2 rub up. And to be fair the finish is very uniform.
  5. Mr White

    1.5mm silicone render, cracking all over

    And btw, this, this sort of conversation I can do. Not the silly insults, accusations of being a ginger. Not having a clue. I can agree to disagree and have an adult conversation, It I will stand by what I said, I thing the op would have benefited from heavily watering down his material on a...
  6. Mr White

    1.5mm silicone render, cracking all over

    Yes, spraying with less water will not go through a hopper gun, it spits. The material is too thick. Hand applying in colder weather neat is ok, 500ml added In the summer in direct sun, while I agree will weaken the material ever so slightly, as with any setting material, will aid in...
  7. Mr White

    1.5mm silicone render, cracking all over

    Why did you say adding 500ml would need a brush to apply?
  8. Mr White

    1.5mm silicone render, cracking all over

    The point was you said it couldn’t be spread by trowel after adding 500ml of water. I quoted you, up there. It would need a brush, you said. Slowing the setting times down on most materials by adding more water will weaken the finished strength of a product, such as concrete........ But...
  9. Mr White

    1.5mm silicone render, cracking all over

    We answering this question sloppy chops or what? Got a shepherds pie and a bottle of hendos waiting here....
  10. Mr White

    1.5mm silicone render, cracking all over

    Like I said, continue to dodge the question and try and move your argument.
  11. Mr White

    1.5mm silicone render, cracking all over

    I’ve answered enough for you, how about explaining why you said watering down silicone by 500ml was no good, need a brush etc. And then apologise to me
  12. Mr White

    1.5mm silicone render, cracking all over

    Answer my question you bellend. Why did you say that 500ml could not be spread by trowel and a brush would be needed. The little video we did shows otherwise? Answer before you get a hernia
  13. Mr White

    1.5mm silicone render, cracking all over

    I’m only a dickhead because I continue to show you up for what you are .......... a t**t A man who come on here to belittle and act a c**t, accuse and throw wild accusations around without evidence, and to act up to the real nuts. Your a phoney, your reputation is f**k*d by a newbie like me...