Used l*m*-g***n solo as my top coat in the end, it's hard work over solid backgrounds but if worked right you can get a really good finish, highly recommended.
Why 3 coats!
No scratch in the scratch coat... What lime did they use, looks like is hasn't cured properly and remained too flexible and soft... What time of year was it done...
The list is endless...
Good morning, names Damon, company Kentish Restoration, based in the corner of Kent, Thanet.
Work mainly on old period properties using traditional materials and methods.
I also have a small, local supply company, Kentish Lime.
Been using it as a base coat on some IWI I'm doing, love the stuff and I do lime work 90% of the time!
That said I haven't top coated, which I plan to be my own mix of fine sand, chalk powder and NHL2...