I would understand that if it was applied in warm weather that this may happen....if you hadn't wet the wall or protected from warm temperatures, but this was only applied in the last week where the temperature was no more than 15 degrees and didn't fall no less than 9 degrees....
This all over the gable wall of the house, near beads and not near beads.....it was machine applied to 18mm and scratched back to leave a finishing coat of 16mm, so depth of render is correct.
Thats why I'm here...was hoping for some guidance. Don't know where to turn to next. The manufacturer says there is nothing wrong with the product, which i believe to be untrue and the client says there is nothing wrong with the blockwork .......who do i turn to now to resolve this?
It wasn't windy and just your normal block......not liteweight. It was pretty much your ideal spray application temperatures. Thats why I'm a bit lost....
This site uses cookies to help personalise content, tailor your experience and to keep you logged in if you register.
By continuing to use this site, you are consenting to our use of cookies.