I've PM a couple of numbers to you.
I've PM a couple of numbers to you.
To provide a good key for floors i use 2 part epoxy seeded with glass frit i also use glass frit in sbr slurries
For rendering yea 1sbr 1 water 1opc 1glass i get my glass frit from virridor near you in st helens near jackson st
For rendering yea 1sbr 1 water 1opc 1glass i get my glass frit from virridor near you in st helens near jackson st
Just brush it on as you would an sbr slurry it privides a better key than sand. glass frit is crushed glass and is usuall sold for fibreglass and glass makingWhat's glass frit? Is it that crushed glass what looks like a sharp/grit sand? Pavers use it round here.That mix, do you trowel it on or brush it on and is it wet on wet or a scratch regards. R